Six, Yin and Yang color
Causes: 1, raw materials have color. 2. The pan head is uneven. 3, the steel buckle is not evenly worn.
Preventive measures: 1, change the hair or change the dish head is not used. 2. Press the disk head hard. 3. Position the weft needle in the middle of the opening.
Seven, jump needle
Reasons for the formation: 1. 2. The position of weft needle and knitting needle is not right.
Preventive measures: 1, the shift needle rod position by the moving needle. 2, the weft needle and knitting in good position, so that all the weft can be hung up.
Eight, easy to dirty belt processing
Causes: 1. The palm filaments are too dirty. 2, all over the belt shaft is too dirty. 3. All places with yarn are not clean enough.
Preventive measures: 1, the accessories room collar facial tissue and chalk, the palm silk piece clean. 2, all over the belt shaft scrub clean. 3, all have yarn through the place, can contact will dye powder factory area scrub clean.
Wave on both sides
Causes: 1, the steel buckle is not evenly worn, the two sides of the small yarn, the middle of the yarn. 2. The steel buckle is too small.
Preventive measures: 1, choose the right steel buckle, according to the normal wear law. 2, steel buckle wear a little suitable, do not wear too big or too little.
Ten, line
Causes: 1, the bottom yarn thick veil. 2, the steel button is not right, the bottom yarn is not covered. 3, steel buckle selection is too thin, each empty thread too much.
Preventive measures: 1, the thicker bottom yarn to the edge, or do not change, add a new. 2, choose the appropriate steel buckle, 1 or 2 groups of piercing method. 3. In general, try to select one group or two groups of puncture, rather than three groups or more.